Abmessung
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mechanisch
Property | Value | Comment |
---|---|---|
Streckgrenze | 160 MPa Show Supplier Material materials with Streckgrenze of 160 MPa | RP02 |
Zugfestigkeit | 160 - 220 MPa Show Supplier Material materials with Zugfestigkeit of 160 - 220 MPa |
Thermisch
Property | Value |
---|
Elektrisch
Property | Value | Comment |
---|---|---|
Korrosionspotenzial | -690 mV Show Supplier Material materials with Korrosionspotenzial of -690 mV | |
spezifischer Widerstand | 3.4e-08 - 4.3e-08 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.4e-08 - 4.3e-08 Ω·m | Changes depending on temper |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Eisen | 0.1 - 0.5 % Show Supplier Material materials with Eisen of 0.1 - 0.5 % |
Kupfer | 0.4 - 0.7 % Show Supplier Material materials with Kupfer of 0.4 - 0.7 % |
Mangan | 1.2 - 1.6 % Show Supplier Material materials with Mangan of 1.2 - 1.6 % |
Silizium | 0.4 - 0.8 % Show Supplier Material materials with Silizium of 0.4 - 0.8 % |
Titan | 0.1 - 0.2 % Show Supplier Material materials with Titan of 0.1 - 0.2 % |
Zink | 0 - 0.1 % Show Supplier Material materials with Zink of 0 - 0.1 % |
Zirkonium | 0 - 0.1 % Show Supplier Material materials with Zirkonium of 0 - 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Processing history | Temper: H24 |