Abmessung
Property | Value |
---|---|
Dimensions | <p>Standard process capabilities:</p> <p>Width: 10-1400mm</p> <p>Thickness 0.050-3.18mm</p> |
Mechanisch
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.36e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.36e-05 1/K | for 20-100°C |
Schmelzpunkt | 642 °C Show Supplier Material materials with Schmelzpunkt of 642 °C | Mean |
Elektrisch
Property | Value | Comment |
---|---|---|
Korrosionspotenzial | -720 mV Show Supplier Material materials with Korrosionspotenzial of -720 mV | |
spezifischer Widerstand | 3.4e-08 - 4.3e-08 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.4e-08 - 4.3e-08 Ω·m | Changes depending on temper |
Chemical properties
Property | Value |
---|---|
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, Heat Exchangers | |
Processing history | Temper: O |