Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.12 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.07200000000000001 GPa Show Supplier Material materials with Biegemodul of 0.07200000000000001 GPa | ASTM D790 |
Dehnung | 490.0 % Show Supplier Material materials with Dehnung of 490.0 % | ASTM D412 |
Härte, Shore A | 90.0 [-] Show Supplier Material materials with Härte, Shore A of 90.0 [-] | ASTM D2240 |
Reißfestigkeit | 176.0 kN/m Show Supplier Material materials with Reißfestigkeit of 176.0 kN/m | ASTM D624 |
Zugfestigkeit | 51.0 MPa Show Supplier Material materials with Zugfestigkeit of 51.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubing and Medical Disposable Applications. |