Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 600.0 % Show Supplier Material materials with Dehnung of 600.0 % | ASTM D412 |
Härte, Shore A | 95.0 [-] Show Supplier Material materials with Härte, Shore A of 95.0 [-] | ASTM D2240 |
Reißfestigkeit | 180.0 kN/m Show Supplier Material materials with Reißfestigkeit of 180.0 kN/m | ASTM D624 |
Zugfestigkeit | 60.0 MPa Show Supplier Material materials with Zugfestigkeit of 60.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods. |