Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.19 g/cm³ Show Supplier Material materials with Dichte of 1.19 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 108.0 MPa Show Supplier Material materials with Biegefestigkeit of 108.0 MPa | ASTM D790 |
Biegemodul | 1.85 GPa Show Supplier Material materials with Biegemodul of 1.85 GPa | ASTM D790 |
Dehnung | 40.0 % Show Supplier Material materials with Dehnung of 40.0 % | ASTM D638 |
Elastizitätsmodul | 1.57 GPa Show Supplier Material materials with Elastizitätsmodul of 1.57 GPa | ASTM D638 |
Härte, Shore D | 81.0 [-] Show Supplier Material materials with Härte, Shore D of 81.0 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 108 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 108 J/m | ASTM D256 |
Zugfestigkeit | 83.0 MPa Show Supplier Material materials with Zugfestigkeit of 83.0 MPa | ASTM D638 |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Electronics, Automotive, Power Tools, Oil-Water Separator, Optics Products. |