Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 450.0 % Show Supplier Material materials with Dehnung of 450.0 % | ASTM D412 | |
Druckverformungsrest | 23 °C | 20 [-] Show Supplier Material materials with Druckverformungsrest of 20 [-] | ASTM D395, for 22hrs |
70 °C | 28 [-] Show Supplier Material materials with Druckverformungsrest of 28 [-] | ASTM D395, for 22hrs | |
Härte, Shore A | 91.0 [-] Show Supplier Material materials with Härte, Shore A of 91.0 [-] | ASTM D2240 | |
Reißfestigkeit | 120.0 kN/m Show Supplier Material materials with Reißfestigkeit of 120.0 kN/m | ASTM D624 | |
Zugfestigkeit | 56.0 MPa Show Supplier Material materials with Zugfestigkeit of 56.0 MPa | ASTM D638 |
Technological properties
Property | ||
---|---|---|
Application areas | Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods. |