Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 580.0 % Show Supplier Material materials with Dehnung of 580.0 % | ASTM D412 | |
Druckverformungsrest | 100 °C | 33 [-] Show Supplier Material materials with Druckverformungsrest of 33 [-] | ASTM D395, for 22hrs |
Härte, Shore A | 90.0 [-] Show Supplier Material materials with Härte, Shore A of 90.0 [-] | ASTM D2240 | |
Reißfestigkeit | 130.0 kN/m Show Supplier Material materials with Reißfestigkeit of 130.0 kN/m | ASTM D624 | |
Zugfestigkeit | 30.0 MPa Show Supplier Material materials with Zugfestigkeit of 30.0 MPa | ASTM D638 |
Technological properties
Property | ||
---|---|---|
Application areas | Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods. |