Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 550.0 % Show Supplier Material materials with Dehnung of 550.0 % | ASTM D412 |
Härte, Shore A | 90.0 [-] Show Supplier Material materials with Härte, Shore A of 90.0 [-] | ASTM D2240 |
Reißfestigkeit | 120.0 kN/m Show Supplier Material materials with Reißfestigkeit of 120.0 kN/m | ASTM D624 |
Zugfestigkeit | 54.0 MPa Show Supplier Material materials with Zugfestigkeit of 54.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Apparel Applications And Outdoor Applications. |