Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.08 g/cm³ Show Supplier Material materials with Dichte of 1.08 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 400.0 % Show Supplier Material materials with Dehnung of 400.0 % | ASTM D412 |
Härte, Shore A | 80.0 [-] Show Supplier Material materials with Härte, Shore A of 80.0 [-] | ASTM D2240 |
Reißfestigkeit | 110.0 kN/m Show Supplier Material materials with Reißfestigkeit of 110.0 kN/m | ASTM D624 |
Zugfestigkeit | 42.0 MPa Show Supplier Material materials with Zugfestigkeit of 42.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Protective Films and Smart Wearable Devices |