Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.028999999999999998 GPa Show Supplier Material materials with Biegemodul of 0.028999999999999998 GPa | ASTM D790 |
Dehnung | 650.0 % Show Supplier Material materials with Dehnung of 650.0 % | ASTM D412 |
Härte, Shore A | 75.0 [-] Show Supplier Material materials with Härte, Shore A of 75.0 [-] | ASTM D2240 |
Reißfestigkeit | 70.0 kN/m Show Supplier Material materials with Reißfestigkeit of 70.0 kN/m | ASTM D624 |
Zugfestigkeit | 31.0 MPa Show Supplier Material materials with Zugfestigkeit of 31.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubing and Medical Disposable Applications. | |
Certifications | Bio-compatibility according to USP class VI |