Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.096 GPa Show Supplier Material materials with Biegemodul of 0.096 GPa | ASTM D790 |
Dehnung | 438.0 % Show Supplier Material materials with Dehnung of 438.0 % | ASTM D412 |
Härte, Shore A | 95.0 [-] Show Supplier Material materials with Härte, Shore A of 95.0 [-] | ASTM D2240 |
Reißfestigkeit | 190.0 kN/m Show Supplier Material materials with Reißfestigkeit of 190.0 kN/m | ASTM D624 |
Zugfestigkeit | 51.0 MPa Show Supplier Material materials with Zugfestigkeit of 51.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubing and Medical Disposable Applications. | |
Certifications | Bio-compatibility according to USP class VI |