Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 1.37 GPa Show Supplier Material materials with Biegemodul of 1.37 GPa | ASTM D790 |
Dehnung | 150.0 % Show Supplier Material materials with Dehnung of 150.0 % | ASTM D412 |
Härte, Shore D | 76.0 [-] Show Supplier Material materials with Härte, Shore D of 76.0 [-] | ASTM D2240 |
Zugfestigkeit | 60.0 MPa Show Supplier Material materials with Zugfestigkeit of 60.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Tubing and Medical Disposable Applications. | |
Certifications | Bio-compatibility according to USP class VI |