Allgemein
Property | Value |
---|---|
Dichte | 1.6 g/cm³ Show Supplier Material materials with Dichte of 1.6 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 270.0 MPa Show Supplier Material materials with Biegefestigkeit of 270.0 MPa | |
Biegemodul | 14.8 GPa Show Supplier Material materials with Biegemodul of 14.8 GPa | |
Dehnung | 2.0 % Show Supplier Material materials with Dehnung of 2.0 % | |
Impact strength, Izod notched, ASTM | 300 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 300 J/m | ASTM D256 |
Zugfestigkeit | 200.0 MPa Show Supplier Material materials with Zugfestigkeit of 200.0 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Parts, Medical equipment, Sports Equipment |