Allgemein
Property | Value |
---|---|
Dichte | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 344.0 MPa Show Supplier Material materials with Biegefestigkeit of 344.0 MPa | |
Biegemodul | 13.739 GPa Show Supplier Material materials with Biegemodul of 13.739 GPa | |
Dehnung | 2.0 % Show Supplier Material materials with Dehnung of 2.0 % | |
Impact strength, Izod notched, ASTM | 400 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 400 J/m | ASTM D256 |
Zugfestigkeit | 216.0 MPa Show Supplier Material materials with Zugfestigkeit of 216.0 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Parts, Sports Equipment |