Allgemein
Property | Value |
---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 166.0 MPa Show Supplier Material materials with Biegefestigkeit of 166.0 MPa | |
Biegemodul | 8.338 GPa Show Supplier Material materials with Biegemodul of 8.338 GPa | |
Dehnung | 2.0 % Show Supplier Material materials with Dehnung of 2.0 % | |
Impact strength, Izod notched, ASTM | 245 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 245 J/m | ASTM D256 |
Zugfestigkeit | 107.0 MPa Show Supplier Material materials with Zugfestigkeit of 107.0 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Parts, Automotive |