Allgemein
Property | Value |
---|---|
Dichte | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 196.0 MPa Show Supplier Material materials with Biegefestigkeit of 196.0 MPa | |
Biegemodul | 10.790999999999999 GPa Show Supplier Material materials with Biegemodul of 10.790999999999999 GPa | |
Dehnung | 2.0 % Show Supplier Material materials with Dehnung of 2.0 % | |
Impact strength, Izod notched, ASTM | 294 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 294 J/m | ASTM D256 |
Zugfestigkeit | 122.0 MPa Show Supplier Material materials with Zugfestigkeit of 122.0 MPa |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical Parts, Automotive |