Allgemein
Property | Value |
---|---|
Dichte | 1.5 g/cm³ Show Supplier Material materials with Dichte of 1.5 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 206.0 MPa Show Supplier Material materials with Biegefestigkeit of 206.0 MPa |
Biegemodul | 6.87 GPa Show Supplier Material materials with Biegemodul of 6.87 GPa |
Impact strength, Izod notched, ASTM | 246 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 246 J/m |
Zugfestigkeit | 157.0 MPa Show Supplier Material materials with Zugfestigkeit of 157.0 MPa |
Thermisch
Property | Value | Pressure | Comment |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 85.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 85.0 °C | 1.8 MPa | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Automotive and Hand Tools. | |
Fillers | 30% Long Glass Fiber |