Allgemein
Property | Value |
---|---|
Dichte | 1.7 g/cm³ Show Supplier Material materials with Dichte of 1.7 g/cm³ |
Mechanisch
Property | Value |
---|---|
Biegefestigkeit | 335.0 MPa Show Supplier Material materials with Biegefestigkeit of 335.0 MPa |
Biegemodul | 13.3 GPa Show Supplier Material materials with Biegemodul of 13.3 GPa |
Impact strength, Izod notched, ASTM | 295 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 295 J/m |
Zugfestigkeit | 222.0 MPa Show Supplier Material materials with Zugfestigkeit of 222.0 MPa |
Thermisch
Property | Value | Pressure | Comment |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 95.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 95.0 °C | 1.8 MPa | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Automotive and Hand Tools. | |
Fillers | 60% Long Glass Fiber |