Allgemein
Property | Value |
---|---|
Dichte | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 192.0 MPa Show Supplier Material materials with Biegefestigkeit of 192.0 MPa | |
Biegemodul | 9.84 GPa Show Supplier Material materials with Biegemodul of 9.84 GPa | |
Impact strength, Izod notched, ASTM | -20 °C | 246 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 246 J/m |
23 °C | 256 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 256 J/m | |
Zugfestigkeit | 108.0 MPa Show Supplier Material materials with Zugfestigkeit of 108.0 MPa |
Thermisch
Property | Value | Pressure | Comment |
---|---|---|---|
Wärmeformbeständigkeitstemperatur | 155.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 155.0 °C | 1.8 MPa | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Car Industry, Frame in the engine bay, Seat frame, Dashboard frame, Frame of Battery base, Door panel, Pedals, Fender apron, Frame of spare tire. Electronics, High precision plug-in/element, Structure parts of the printer, Frame of the 3C products, Structure parts. Petrochemical, Corrosion and abrasion resistance parts, Grille platform, Parts of filtration facility, Reactor parts. Others, Seat frame of bicycle, Snowboard, Structure parts of the exercise gear and pedals, Toe of Safety boot, Safety helmet. | |
Fillers | 50% Glass Fiber |