Property | Value | Comment |
---|---|---|
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 67.0 MPa Show Supplier Material materials with Biegefestigkeit of 67.0 MPa | ASTM D790 |
Biegemodul | 2.45 GPa Show Supplier Material materials with Biegemodul of 2.45 GPa | ASTM D790 |
Hardness, Rockwell R | 119.0 [-] Show Supplier Material materials with Hardness, Rockwell R of 119.0 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 245 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 245 J/m | ASTM D256 |
Streckgrenze | 38.0 MPa Show Supplier Material materials with Streckgrenze of 38.0 MPa | ASTM D638 |
Zugfestigkeit | 34.0 MPa Show Supplier Material materials with Zugfestigkeit of 34.0 MPa | ASTM D638 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Vicat-Erweichungstemperatur | 102.0 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 102.0 °C | ASTM D1525, 1kg load | |||
Wärmeformbeständigkeitstemperatur | 85.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 85.0 °C | 1.8 MPa | ASTM D648 | ||
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 40.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 40.0 g/10min | ASTM D1238, 220°C,10kg/cm2 |
Technological properties
Property | ||
---|---|---|
Application areas | Tv-housing, Large or Complex shaped products, Air conditioners |