Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.03 g/cm³ Show Supplier Material materials with Dichte of 1.03 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 60.0 MPa Show Supplier Material materials with Biegefestigkeit of 60.0 MPa | ASTM D790 |
Hardness, Rockwell R | 100.0 [-] Show Supplier Material materials with Hardness, Rockwell R of 100.0 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 392 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 392 J/m | ASTM D256 |
Streckgrenze | 35.0 MPa Show Supplier Material materials with Streckgrenze of 35.0 MPa | ASTM D638 |
Zugfestigkeit | 30.0 MPa Show Supplier Material materials with Zugfestigkeit of 30.0 MPa | ASTM D638 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Wärmeformbeständigkeitstemperatur | 85.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 85.0 °C | 1.8 MPa | ASTM D648 | ||
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 5.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 5.0 g/10min | ASTM D1238, 220°C,10kg/cm2 |
Technological properties
Property | ||
---|---|---|
Application areas | Tool boxes, Motorcycle parts, Helmets, Extruded sheet and profile |