Property | Value | Comment |
---|---|---|
Dichte | 1.16 g/cm³ Show Supplier Material materials with Dichte of 1.16 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 70.0 MPa Show Supplier Material materials with Biegefestigkeit of 70.0 MPa | ASTM D790 |
Biegemodul | 1.96 GPa Show Supplier Material materials with Biegemodul of 1.96 GPa | ASTM D790 |
Impact strength, Izod notched, ASTM | 215.2 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 215.2 J/m | ASTM D256 |
Streckgrenze | 43.5 MPa Show Supplier Material materials with Streckgrenze of 43.5 MPa | ASTM D638 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Vicat-Erweichungstemperatur | 95.0 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 95.0 °C | ASTM D1525, 1kg load | |||
Wärmeformbeständigkeitstemperatur | 79.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 79.0 °C | 1.8 MPa | ASTM D648 | ||
Entflammbarkeit | UL94 V0 (2.5mm) |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 45.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 45.0 g/10min | ASTM D1238, 220°C,10kg/cm2 |
Technological properties
Property | ||
---|---|---|
Application areas | Telephone housing, Tv housing |