Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 80.0 MPa Show Supplier Material materials with Biegefestigkeit of 80.0 MPa | ASTM D790 |
Biegemodul | 2.31 GPa Show Supplier Material materials with Biegemodul of 2.31 GPa | ASTM D790 |
Hardness, Rockwell R | 113.0 [-] Show Supplier Material materials with Hardness, Rockwell R of 113.0 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 98 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 98 J/m | ASTM D256 |
Streckgrenze | 52.0 MPa Show Supplier Material materials with Streckgrenze of 52.0 MPa | ASTM D638 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Wärmeformbeständigkeitstemperatur | 83.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 83.0 °C | 1.8 MPa | ASTM D648 | ||
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 21.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 21.0 g/10min | ASTM D1238, 220°C,10kg/cm2 |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic appliances, Air conditioner, Panel, Humidifier water tank |