Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 85.0 MPa Show Supplier Material materials with Biegefestigkeit of 85.0 MPa | ASTM D790 |
Biegemodul | 2.13 GPa Show Supplier Material materials with Biegemodul of 2.13 GPa | ASTM D790 |
Hardness, Rockwell R | 70.0 [-] Show Supplier Material materials with Hardness, Rockwell R of 70.0 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 637 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 637 J/m | ASTM D256 |
Streckgrenze | 53.0 MPa Show Supplier Material materials with Streckgrenze of 53.0 MPa | ASTM D638 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Wärmeformbeständigkeitstemperatur | 88.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 88.0 °C | 1.8 MPa | ASTM D648 | ||
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 15.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 15.0 g/10min | ASTM D1238, 260°C,2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automibile interior parts, Consumer electronic products, General molding products |