Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 84.5 MPa Show Supplier Material materials with Biegefestigkeit of 84.5 MPa | ASTM D790 |
Biegemodul | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ASTM D790 |
Hardness, Rockwell R | 118.0 [-] Show Supplier Material materials with Hardness, Rockwell R of 118.0 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 490 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 490 J/m | ASTM D256 |
Streckgrenze | 58.0 MPa Show Supplier Material materials with Streckgrenze of 58.0 MPa | ASTM D638 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Vicat-Erweichungstemperatur | 110.0 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 110.0 °C | ASTM D1525, 1kg load | |||
Wärmeformbeständigkeitstemperatur | 93.0 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 93.0 °C | 1.8 MPa | ASTM D648 | ||
Entflammbarkeit | UL94 V0 (3.2-3.5mm) |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 20.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 20.0 g/10min | ASTM D1238, 260°C,2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automibile interior parts, Consumer electronic products, General molding products |