Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 950.0 % Show Supplier Material materials with Dehnung of 950.0 % | ASTM D412 |
Härte, Shore A | 45.0 [-] Show Supplier Material materials with Härte, Shore A of 45.0 [-] | ASTM D2240 |
Reißfestigkeit | 28.0 kN/m Show Supplier Material materials with Reißfestigkeit of 28.0 kN/m | ASTM D624 |
Zugfestigkeit | 10.0 MPa Show Supplier Material materials with Zugfestigkeit of 10.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Synthetic Leather, Furniture, Sports and Recreations. |