Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 750.0 % Show Supplier Material materials with Dehnung of 750.0 % | ASTM D412 |
Härte, Shore A | 62.0 [-] Show Supplier Material materials with Härte, Shore A of 62.0 [-] | ASTM D2240 |
Reißfestigkeit | 49.0 kN/m Show Supplier Material materials with Reißfestigkeit of 49.0 kN/m | ASTM D624 |
Zugfestigkeit | 18.0 MPa Show Supplier Material materials with Zugfestigkeit of 18.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Synthetic Leather, Furniture, Sports and Recreations. |