Property | Value | Comment |
---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 550.0 % Show Supplier Material materials with Dehnung of 550.0 % | ASTM D412 |
Härte, Shore A | 85.0 [-] Show Supplier Material materials with Härte, Shore A of 85.0 [-] | ASTM D2240 |
Reißfestigkeit | 88.0 kN/m Show Supplier Material materials with Reißfestigkeit of 88.0 kN/m | ASTM D624 |
Zugfestigkeit | 33.0 MPa Show Supplier Material materials with Zugfestigkeit of 33.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Synthetic Leather, Furniture, Sports and Recreations. |