Property | Value | Comment |
---|---|---|
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 800.0 % Show Supplier Material materials with Dehnung of 800.0 % | ASTM D412 |
Härte, Shore A | 65.0 [-] Show Supplier Material materials with Härte, Shore A of 65.0 [-] | ASTM D2240 |
Reißfestigkeit | 42.0 kN/m Show Supplier Material materials with Reißfestigkeit of 42.0 kN/m | ASTM D624 |
Zugfestigkeit | 15.0 MPa Show Supplier Material materials with Zugfestigkeit of 15.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Synthetic Leather, Furniture, Sports and Recreations. |