Allgemein
Property | Value | Comment |
---|---|---|
Bio-based content | 46.0 % Show Supplier Material materials with Bio-based content of 46.0 % | |
Dichte | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 1100.0 % Show Supplier Material materials with Dehnung of 1100.0 % | ASTM D412 |
Härte, Shore A | 75.0 [-] Show Supplier Material materials with Härte, Shore A of 75.0 [-] | ASTM D2240 |
Reißfestigkeit | 100.0 kN/m Show Supplier Material materials with Reißfestigkeit of 100.0 kN/m | ASTM D624 |
Zugfestigkeit | 15.0 MPa Show Supplier Material materials with Zugfestigkeit of 15.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |