Allgemein
Property | Value | Comment |
---|---|---|
Bio-based content | 28.0 % Show Supplier Material materials with Bio-based content of 28.0 % | |
Dichte | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 750.0 % Show Supplier Material materials with Dehnung of 750.0 % | ASTM D412 |
Härte, Shore A | 83.0 [-] Show Supplier Material materials with Härte, Shore A of 83.0 [-] | ASTM D2240 |
Reißfestigkeit | 115.0 kN/m Show Supplier Material materials with Reißfestigkeit of 115.0 kN/m | ASTM D624 |
Zugfestigkeit | 23.0 MPa Show Supplier Material materials with Zugfestigkeit of 23.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |