Allgemein
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 900.0 % Show Supplier Material materials with Dehnung of 900.0 % | ASTM D412 |
Härte, Shore A | 75.0 [-] Show Supplier Material materials with Härte, Shore A of 75.0 [-] | ASTM D2240 |
Reißfestigkeit | 110.0 kN/m Show Supplier Material materials with Reißfestigkeit of 110.0 kN/m | ASTM D624 |
Zugfestigkeit | 19.0 MPa Show Supplier Material materials with Zugfestigkeit of 19.0 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Packaging Material, Footwear, Consumer Goods, Automotive |