Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Dichte of 1.47 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | ISO527 |
Elastizitätsmodul | 23.0 °C | 11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | ISO527 |
Härte, Shore D | 23.0 °C | 82 [-] Show Supplier Material materials with Härte, Shore D of 82 [-] | ISO868 |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | ISO179 |
23.0 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | ISO179 | |
Schlagzähigkeit, Charpy ungekerbt | -30.0 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | ISO179 |
23.0 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | ISO179 | |
Zugfestigkeit | 23.0 °C | 160 MPa Show Supplier Material materials with Zugfestigkeit of 160 MPa | ISO527 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 165 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 165 °C | ISO75/A |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing connection; Automotive lightweight components; Sport health equipment | |
Fillers | 50% Glass Fiber | |
Processing methods | Drying Temperature: 80-85°C, Drying Time: 3-4 hr, Rear Temperature: 190°C, Middle Temperature: 210°C, Front Temperature: 220°C, Nozzle Temperature: 210°C, Mold Temperature: 40-60°C, Injection Pressure: 80-100 MPa |