Allgemein
Property | Value |
---|---|
Recycled Content | 100 % Show Supplier Material materials with Recycled Content of 100 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 5.34 - 6.26 GPa Show Supplier Material materials with Biegemodul of 5.34 - 6.26 GPa | |
Dehnung | 23.0 °C | 4 - 6 % Show Supplier Material materials with Dehnung of 4 - 6 % | |
Elastizitätsmodul | 23.0 °C | 5.7 - 6.7 GPa Show Supplier Material materials with Elastizitätsmodul of 5.7 - 6.7 GPa | ISO 527-1,-2 |
Flexural yield strength | 23.0 °C | 95 - 100 MPa Show Supplier Material materials with Flexural yield strength of 95 - 100 MPa | ISO 178 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 30 - 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 30 - 40 kJ/m² | ISO 179 |
Streckgrenze | 23.0 °C | 65 - 80 MPa Show Supplier Material materials with Streckgrenze of 65 - 80 MPa |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 9 - 15 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9 - 15 g/10min | 230°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, household appliances, furniture, construction, fitting, industrial injection. Design of products tailored to customer requirements. | |
Color | Black, Natural | |
Fillers | 37-43% Glass Fiber |