Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.9 - 0.92 g/cm³ Show Supplier Material materials with Dichte of 0.9 - 0.92 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | max., ISO 787/2 |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Aschegehalt | 23.0 °C | 3 % Show Supplier Material materials with Aschegehalt of 3 % | max., ISO 3451-1, A |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 0.3 - 0.6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 0.3 - 0.6 cm³/10min | 190°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Construction, industrial & silage films, bags, hoods & sacks, injection moulding, irrigation pipes, corrugated tubing, etc. | |
Color | Natural |