Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 - 1.06 g/cm³ Show Supplier Material materials with Dichte of 1.02 - 1.06 g/cm³ | ISO 1183-1, A |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.35 - 1.65 GPa Show Supplier Material materials with Biegemodul of 1.35 - 1.65 GPa | ISO 178 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 30 - 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 30 - 40 kJ/m² | ISO 179 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 3 - 6 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 3 - 6 g/10min | 230°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Injection Moulding | |
Color | Black | |
Fillers | 17-23% Ultrafine Talc |