Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.08 - 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.08 - 1.12 g/cm³ | ISO 1183-1, A |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.8 - 2.2 GPa Show Supplier Material materials with Biegemodul of 1.8 - 2.2 GPa | ISO 178 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 25 - 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 25 - 35 kJ/m² | ISO 179 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 9 - 14 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9 - 14 g/10min | 230°C/2.16kg, ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Injection Moulding | |
Color | Black, Natural | |
Fillers | 27-33% Ultrafine Talc |