Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.6 g/cm³ Show Supplier Material materials with Dichte of 1.6 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % |
Elastizitätsmodul | 23.0 °C | 240 GPa Show Supplier Material materials with Elastizitätsmodul of 240 GPa |
Poissonzahl | 23.0 °C | 0.25 [-] Show Supplier Material materials with Poissonzahl of 0.25 [-] |
Scherfestigkeit | 23.0 °C | 40 MPa Show Supplier Material materials with Scherfestigkeit of 40 MPa |
Zugfestigkeit | 23.0 °C | 3400 MPa Show Supplier Material materials with Zugfestigkeit of 3400 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 68% Carbon Fiber | |
Processing methods | The production process is formed by laminating hot-pressed carbon fiber prepreg. |