Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-42 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % |
Elastizitätsmodul | 23.0 °C | 145 GPa Show Supplier Material materials with Elastizitätsmodul of 145 GPa |
Härte, Brinell | 23.0 °C | 160 [-] Show Supplier Material materials with Härte, Brinell of 160 [-] |
Härte, Rockwell C | 23.0 °C | 3 [-] Show Supplier Material materials with Härte, Rockwell C of 3 [-] |
Härte, Vickers | 23.0 °C | 160 [-] Show Supplier Material materials with Härte, Vickers of 160 [-] |
Streckgrenze | 23.0 °C | 600 MPa Show Supplier Material materials with Streckgrenze of 600 MPa |
Zugfestigkeit | 23.0 °C | 550 - 750 MPa Show Supplier Material materials with Zugfestigkeit of 550 - 750 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.72E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.72E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 22 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: High performance precision mechanical parts, high end screws, optical fibre connectors | |
Corrosion properties | Corrosion resistance rating: 5 out of 5 | |
General machinability | Machinability: 60-80 % | |
Processing history | Condition: H14 |