Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-35 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % |
Elastizitätsmodul | 23.0 °C | 165 GPa Show Supplier Material materials with Elastizitätsmodul of 165 GPa |
Härte, Brinell | 23.0 °C | 137 [-] Show Supplier Material materials with Härte, Brinell of 137 [-] |
Härte, Rockwell C | 23.0 °C | 0 [-] Show Supplier Material materials with Härte, Rockwell C of 0 [-] |
Härte, Vickers | 23.0 °C | 140 [-] Show Supplier Material materials with Härte, Vickers of 140 [-] |
Streckgrenze | 23.0 °C | 300 MPa Show Supplier Material materials with Streckgrenze of 300 MPa |
Zugfestigkeit | 23.0 °C | 500 MPa Show Supplier Material materials with Zugfestigkeit of 500 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.72E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.72E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 22.5 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 22.5 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 2.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Mechanical parts in very demanding environments | |
Corrosion properties | Corrosion resistance rating: 5 out of 5 | |
General machinability | Machinability: 40 % | |
Processing history | Condition: O |