Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Dichte of 8.3 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-20 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 32 % Show Supplier Material materials with Dehnung of 32 % |
Elastizitätsmodul | 23.0 °C | 115 GPa Show Supplier Material materials with Elastizitätsmodul of 115 GPa |
Härte, Brinell | 23.0 °C | 76 [-] Show Supplier Material materials with Härte, Brinell of 76 [-] |
Härte, Rockwell C | 23.0 °C | 0 [-] Show Supplier Material materials with Härte, Rockwell C of 0 [-] |
Härte, Vickers | 23.0 °C | 80 [-] Show Supplier Material materials with Härte, Vickers of 80 [-] |
Streckgrenze | 23.0 °C | 180 MPa Show Supplier Material materials with Streckgrenze of 180 MPa |
Zugfestigkeit | 23.0 °C | 240 MPa Show Supplier Material materials with Zugfestigkeit of 240 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 380 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 380 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 4.90E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 4.90E+7 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Electrical and electronic contacts, screws, for high performance relaxation | |
Corrosion properties | Corrosion resistance rating: 3 out of 5 | |
General machinability | Machinability: 60 % | |
Processing history | Condition: O |