Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 30 - 40 % Show Supplier Material materials with Dehnung of 30 - 40 % |
Elastizitätsmodul | 23.0 °C | 124 GPa Show Supplier Material materials with Elastizitätsmodul of 124 GPa |
Härte, Brinell | 23.0 °C | 160 - 210 [-] Show Supplier Material materials with Härte, Brinell of 160 - 210 [-] |
Härte, Rockwell C | 23.0 °C | 3 - 17 [-] Show Supplier Material materials with Härte, Rockwell C of 3 - 17 [-] |
Härte, Vickers | 23.0 °C | 160 - 210 [-] Show Supplier Material materials with Härte, Vickers of 160 - 210 [-] |
Streckgrenze | 23.0 °C | 300 - 550 MPa Show Supplier Material materials with Streckgrenze of 300 - 550 MPa |
Zugfestigkeit | 23.0 °C | 570 - 670 MPa Show Supplier Material materials with Zugfestigkeit of 570 - 670 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 45 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 45 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.01 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.01 [-] | max |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Cryogenic fittings, electrical connectors, rods and couplings, food industry, bolts, valves | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
Friction | Friction behavior rating: 4 out of 5 | |
General machinability | Machinability: 60 % |