Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.6 g/cm³ Show Supplier Material materials with Dichte of 7.6 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 20 - 32 % Show Supplier Material materials with Dehnung of 20 - 32 % |
Elastizitätsmodul | 23.0 °C | 116 GPa Show Supplier Material materials with Elastizitätsmodul of 116 GPa |
Härte, Brinell | 23.0 °C | 155 - 190 [-] Show Supplier Material materials with Härte, Brinell of 155 - 190 [-] |
Härte, Rockwell C | 23.0 °C | 1 - 13 [-] Show Supplier Material materials with Härte, Rockwell C of 1 - 13 [-] |
Härte, Vickers | 23.0 °C | 152 - 186 [-] Show Supplier Material materials with Härte, Vickers of 152 - 186 [-] |
Streckgrenze | 23.0 °C | 300 - 450 MPa Show Supplier Material materials with Streckgrenze of 300 - 450 MPa |
Zugfestigkeit | 23.0 °C | 600 - 700 MPa Show Supplier Material materials with Zugfestigkeit of 600 - 700 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 54 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 54 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 7.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 7.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.15 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.15 [-] |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
Friction | Friction behavior rating: 4 out of 5 | |
General machinability | Machinability: 50 % |