Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Supplier Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-14 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 11 % Show Supplier Material materials with Dehnung of 11 % |
Elastizitätsmodul | 23.0 °C | 115 GPa Show Supplier Material materials with Elastizitätsmodul of 115 GPa |
Härte, Brinell | 23.0 °C | 290 - 314 [-] Show Supplier Material materials with Härte, Brinell of 290 - 314 [-] |
Härte, Rockwell C | 23.0 °C | 31 - 34 [-] Show Supplier Material materials with Härte, Rockwell C of 31 - 34 [-] |
Härte, Vickers | 23.0 °C | 300 - 330 [-] Show Supplier Material materials with Härte, Vickers of 300 - 330 [-] |
Streckgrenze | 23.0 °C | 910 - 1000 MPa Show Supplier Material materials with Streckgrenze of 910 - 1000 MPa |
Zugfestigkeit | 23.0 °C | 950 - 1100 MPa Show Supplier Material materials with Zugfestigkeit of 950 - 1100 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.72E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.72E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 8.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 8.00E+6 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Connectors, precision mechanical & electrical parts | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
General machinability | Machinability: 60 % | |