Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): 1-20 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % |
Elastizitätsmodul | 23.0 °C | 100 GPa Show Supplier Material materials with Elastizitätsmodul of 100 GPa |
Härte, Brinell | 23.0 °C | 103 - 166 [-] Show Supplier Material materials with Härte, Brinell of 103 - 166 [-] |
Härte, Rockwell C | 23.0 °C | 0 - 5 [-] Show Supplier Material materials with Härte, Rockwell C of 0 - 5 [-] |
Härte, Vickers | 23.0 °C | 110 - 170 [-] Show Supplier Material materials with Härte, Vickers of 110 - 170 [-] |
Streckgrenze | 23.0 °C | 250 - 400 MPa Show Supplier Material materials with Streckgrenze of 250 - 400 MPa |
Zugfestigkeit | 23.0 °C | 450 - 600 MPa Show Supplier Material materials with Zugfestigkeit of 450 - 600 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.1E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 113 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 113 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 1.50E+7 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 1.50E+7 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Machined parts for optical and electronic industry, RoHS compliant | |
Corrosion properties | Corrosion resistance rating: 3 out of 5 | |
General machinability | Machinability: 70 % | |
Processing history | Condition: H14 |