Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Supplier Material materials with Dichte of 8.95 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 18 % Show Supplier Material materials with Dehnung of 18 % |
Elastizitätsmodul | 23.0 °C | 128 - 144 GPa Show Supplier Material materials with Elastizitätsmodul of 128 - 144 GPa |
Härte, Brinell | 23.0 °C | 199 [-] Show Supplier Material materials with Härte, Brinell of 199 [-] |
Härte, Rockwell C | 23.0 °C | 15 [-] Show Supplier Material materials with Härte, Rockwell C of 15 [-] |
Härte, Vickers | 23.0 °C | 199 [-] Show Supplier Material materials with Härte, Vickers of 199 [-] |
Streckgrenze | 23.0 °C | 655 MPa Show Supplier Material materials with Streckgrenze of 655 MPa |
Zugfestigkeit | 23.0 °C | 725 - 730 MPa Show Supplier Material materials with Zugfestigkeit of 725 - 730 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.64E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.64E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 38 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 38 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1 [-] | max |
Technological properties
Property | ||
---|---|---|
Application areas | Hardiall® can be an alternative to Beryllium Copper for some applications. It is environment friendly, being Beryllium-free, Lead-free, and recyclable. Aerospace: friction bushings and bearings. In landing gears, bushings and bearings are required to operate under severe conditions, they need to be lubricated and replaced frequently causing recurring maintenance downtimes. To reduce maintenance costs, Hardiall® is used for such applications as it demonstrates excellent lubricity, wear, and galling resistance. Oil & Gas: couplings for onshore production systems e.g. sucker rods. Hardiall is also used in onshore oil pumps as sucker rod and valve rod guide bushing couplings. In such applications where stainless steel is generally used, Hardiall® demonstrates excellent resistance to metal-to-metal wear. Mining: bushings and bearings. In Mining equipment, bushings and bearings are highly solicited components. They need to be lubricated and replaced frequently implying recurrent production downtimes and maintenance man hours. Hardiall® is used in excavators, mining trucks and longwall shearers. | |
Corrosion properties | Corrosion resistance rating: 5 out of 5 | |
Friction | Friction behavior rating: 5 out of 5 | |
General machinability | Machinability: 60 % | |
Processing history | Condition: TS |