Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.6 g/cm³ Show Supplier Material materials with Dichte of 7.6 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): 76,2-254 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % |
Elastizitätsmodul | 23.0 °C | 125 GPa Show Supplier Material materials with Elastizitätsmodul of 125 GPa |
Härte, Brinell | 23.0 °C | 187 - 241 [-] Show Supplier Material materials with Härte, Brinell of 187 - 241 [-] |
Härte, Rockwell C | 23.0 °C | 11 - 24 [-] Show Supplier Material materials with Härte, Rockwell C of 11 - 24 [-] |
Härte, Vickers | 23.0 °C | 184 - 247 [-] Show Supplier Material materials with Härte, Vickers of 184 - 247 [-] |
Streckgrenze | 23.0 °C | 345 MPa Show Supplier Material materials with Streckgrenze of 345 MPa |
Zugfestigkeit | 23.0 °C | 689 MPa Show Supplier Material materials with Zugfestigkeit of 689 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 40 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 40 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.5 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.5 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Aerospace industry: rings, bushings and bearings for landing gears; Marine industry: distributor bodies, screws, forged parts | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
Friction | Friction behavior rating: 4 out of 5 | |
General machinability | Machinability: 30 % | |
Processing history | Condition: HR50, TQ50 |