Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.5 g/cm³ Show Supplier Material materials with Dichte of 7.5 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 8 % Show Supplier Material materials with Dehnung of 8 % |
Elastizitätsmodul | 23.0 °C | 125 GPa Show Supplier Material materials with Elastizitätsmodul of 125 GPa |
Härte, Brinell | 23.0 °C | 185 [-] Show Supplier Material materials with Härte, Brinell of 185 [-] |
Härte, Rockwell C | 23.0 °C | 12 [-] Show Supplier Material materials with Härte, Rockwell C of 12 [-] |
Härte, Vickers | 23.0 °C | 185 [-] Show Supplier Material materials with Härte, Vickers of 185 [-] |
Streckgrenze | 23.0 °C | 390 MPa Show Supplier Material materials with Streckgrenze of 390 MPa |
Zugfestigkeit | 23.0 °C | 740 MPa Show Supplier Material materials with Zugfestigkeit of 740 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 40 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 40 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.5 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.5 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace industry: rings, bushings and bearings for landing gears, mechanical parts; Hydraulic industry: pump blocks | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
Friction | Friction behavior rating: 4 out of 5 | |
General machinability | Machinability: 40 % |