Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Available size round products (mm): up to 12 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Supplier Material materials with Elastizitätsmodul of 120 GPa |
Härte, Brinell | 23.0 °C | 230 [-] Show Supplier Material materials with Härte, Brinell of 230 [-] |
Härte, Rockwell C | 23.0 °C | 22 [-] Show Supplier Material materials with Härte, Rockwell C of 22 [-] |
Härte, Vickers | 23.0 °C | 235 [-] Show Supplier Material materials with Härte, Vickers of 235 [-] |
Streckgrenze | 23.0 °C | 700 MPa Show Supplier Material materials with Streckgrenze of 700 MPa |
Zugfestigkeit | 23.0 °C | 780 - 880 MPa Show Supplier Material materials with Zugfestigkeit of 780 - 880 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.62E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 52 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 52 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 8.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 8.00E+6 S/m |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 1.01 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 1.01 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Niclafor can be a substitute to Copper-Titanium and Copper-Beryllium for some applications. It used in the automotive industry, for example on bushings and bearings, eg. small end rings in high performance car engines. Niclafor® is also a material of reference in the eyewear industry: its high elasticity and formability allow light and durable designs. Niclafor® is extensively used in the electronics industry, including aerospace systems, for applications such as EMI shielding and connector parts. Summary of typical applications: Electronics (Relays, EMI Shielding, etc.), Connectors, Electrical engineering, Automotive, Telecom and Mobile phones, Eyewear and Spectacles industry, Domestic appliance. | |
Corrosion properties | Corrosion resistance rating: 4 out of 5 | |
General machinability | Machinability: 45 % | |
Processing history | Condition: TD4 |