Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.6 g/cm³ Show Supplier Material materials with Dichte of 8.6 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 12 % Show Supplier Material materials with Dehnung of 12 % |
Elastizitätsmodul | 23.0 °C | 110 GPa Show Supplier Material materials with Elastizitätsmodul of 110 GPa |
Härte, Brinell | 23.0 °C | 150 [-] Show Supplier Material materials with Härte, Brinell of 150 [-] |
Härte, Rockwell C | 23.0 °C | 0 [-] Show Supplier Material materials with Härte, Rockwell C of 0 [-] |
Härte, Vickers | 23.0 °C | 149 [-] Show Supplier Material materials with Härte, Vickers of 149 [-] |
Streckgrenze | 23.0 °C | 340 MPa Show Supplier Material materials with Streckgrenze of 340 MPa |
Zugfestigkeit | 23.0 °C | 540 MPa Show Supplier Material materials with Zugfestigkeit of 540 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.75E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | for 20-200°C |
Wärmeleitfähigkeit | 23.0 °C | 30 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 30 W/(m·K) | for 20-200°C |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 5.00E+6 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Technological properties
Property | ||
---|---|---|
Application areas | Summary of typical applications: Bearing cages, rotor bars for engines, valve guides | |
Corrosion properties | Corrosion resistance rating: 3 out of 5 | |
Friction | Friction behavior rating: 5 out of 5 | |
General machinability | Machinability: 30 % | |
Processing history | Condition: H |